Fiber and non-woven fabric

Fiber and non-woven fabric

Caractéristiques du produit

Fiber grade polylactic acid chips have narrow relative molecular weight distribution, low impurity content, and good fiber forming properties. Through extrusion and stretching equipment, short fibers and different specifications of filament can be produced. Polylactic acid short fibers can be used as fillers, as well as in pure or blended spinning, and can also be used for the production of hot air, hot rolled, spunlaced, and needle punched non-woven fabrics. Polylactic acid fibers have the characteristics of both chemical fibers and bio based fibers, with excellent mechanical properties, skin friendliness, drape resistance, antibacterial and mold resistance, as well as high resilience. They are widely used in fields such as clothing, bedding, daily life, medical and health care.

Hotline de service 24 heures

0086-514-82800752

Contact +
PRODUCT
Numéro de marque du produit

HT201

Short fiber, filament

Low melting point, high melting point, suitable for low shrinkage, high-strength fibers

HT301

Short fiber, filament, non-woven fabric, monofilament

Moderate melting point, high melting point, excellent fiber forming ability and low shrinkage

HT302

nonwovens

Moderate melting point and melting point, with excellent spinning viscosity

HT305

nonwovens

Moderate melting point and low melting point, suitable for low melting point layers in skin core composite fiber structures


Applications typiques
Applications typiques

Clothing: women's shirts, men's and women's outerwear, pajamas, sweaters, T-shirts, long and short sleeved shirts, underwear, socks, sportswear, and pet products;

Bedding: bedding, pillowcases, bed sheets, bed covers, mosquito nets, etc;

Decoration: sand cloth, furniture cloth, curtain cloth, etc;

Industrial use: nets or ropes, etc.

Stockage et traitement
Stockage et traitement

Polylactic acid resin should be stored below 50 ℃.

The moisture content of spinning chips should be less than 50ppm, preferably less than 30ppm;

Suggested processing temperature ≤ 230 ℃.


Application